Kynar Flex® 3120-50 America

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® resins are fluorinated thermoplastic copolymers.

Kynar Flex® 3120-50 is a pelletized flexible, semi-crystalline VF2 based copolymer. It can be molded or extruded and has a useful temperature range from -40°C-150°C. Kynar Flex® 3120-50 has a UL RTI of 150°C.

Kynar Flex® 3120-50 can be used in compounding for cross-linkable wire and cable as well as both wire applications requiring low temperature flexibility and high temperature resistance.

Kynar Flex® 3120-50 also finds use as a polymer processing aid (PPA) for polyolefins. The use of Kynar Flex® 3120-50 or Kynar Flex 3121-50 at 200 -1000 ppm levels reduces extruder pressure, improves surface finish, reduces die build up, and improves gauge control.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Abrasion resistance, weight loss

16 - 19 mg

Show Supplier Material materials with Abrasion resistance, weight loss of 16 - 19 mg

ASTM-G195-13A, CS 17 1000g:pad, 1000 cycles

Coefficient of friction, kinetic

0.3 [-]

Show Supplier Material materials with Coefficient of friction, kinetic of 0.3 [-]

ASTM D1894, vs Steel

Coefficient of friction, static

0.31 [-]

Show Supplier Material materials with Coefficient of friction, static of 0.31 [-]

ASTM D1894, vs Steel

Density

23.0 °C

1.75 - 1.77 g/cm³

Show Supplier Material materials with Density of 1.75 - 1.77 g/cm³

ASTM D792

Limiting oxygen index

23.0 °C

42 %

Show Supplier Material materials with Limiting oxygen index of 42 %

ASTM D2863

Water absorption

23.0 °C

0.03 - 0.05 %

Show Supplier Material materials with Water absorption of 0.03 - 0.05 %

ASTM D570

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

31 - 41.4 MPa

Show Supplier Material materials with Compressive strength of 31 - 41.4 MPa

ASTM D695

Elastic modulus

23.0 °C

0.69 - 1.17 GPa

Show Supplier Material materials with Elastic modulus of 0.69 - 1.17 GPa

ASTM D638

Elongation

23.0 °C

300 - 500 %

Show Supplier Material materials with Elongation of 300 - 500 %

ASTM D638

Elongation at yield

23.0 °C

10 - 20 %

Show Supplier Material materials with Elongation at yield of 10 - 20 %

ASTM D638

Flexural modulus

23.0 °C

0.62 - 0.83 GPa

Show Supplier Material materials with Flexural modulus of 0.62 - 0.83 GPa

ASTM D790

Hardness, Shore D

23.0 °C

65 - 70 [-]

Show Supplier Material materials with Hardness, Shore D of 65 - 70 [-]

ASTM D2240

Tensile strength

23.0 °C

34.5 - 48.3 MPa

Show Supplier Material materials with Tensile strength of 34.5 - 48.3 MPa

ASTM D638

Yield strength

23.0 °C

24.1 - 34.5 MPa

Show Supplier Material materials with Yield strength of 24.1 - 34.5 MPa

ASTM D638

Impact strength, Charpy notched, ASTM

No Break @ 23°C, ASTM D256

Impact strength, Charpy unnotched, ASTM

No Break @ 23°C, ASTM D256

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.26E-4 - 1.85E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.26E-4 - 1.85E-4 1/K

ASTM D696

Glass transition temperature

-41.1 - -39.4 °C

Show Supplier Material materials with Glass transition temperature of -41.1 - -39.4 °C

ASTM D7028

Heat deflection temperature, 0.45 MPa

54.4 - 76.7 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 54.4 - 76.7 °C

ASTM D648, 248 °F/hr

Heat deflection temperature, 1.80 MPa

43.3 - 54.4 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 43.3 - 54.4 °C

ASTM D648, 248 °F/hr

Melting point

161 - 168 °C

Show Supplier Material materials with Melting point of 161 - 168 °C

ASTM D3418

Relative temperature index, electrical

150 °C

Show Supplier Material materials with Relative temperature index, electrical of 150 °C

UL 746B

Relative temperature index, mechanical strength

150 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C

UL 746B

Specific heat capacity

23.0 °C

745 - 958 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 745 - 958 J/(kg·K)

DSC

Thermal conductivity

23.0 °C

0.14 - 0.18 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.14 - 0.18 W/(m·K)

ASTM D433

Thermal decomposition in air

375 °C

Show Supplier Material materials with Thermal decomposition in air of 375 °C

TGA, 1% wt. loss

Thermal decomposition in nitrogen

410 °C

Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C

TGA, 1% wt. loss

Flammability

At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 1 IEC 60695-11-10: V-0 and yellow card available, 5V at thickness 1 mm IEC 60695-11-20: 5VA

Electrical

PropertyTemperatureValueComment

Dielectric constant, 1KHz

23.0 °C

3.2 - 10.2 [-]

Show Supplier Material materials with Dielectric constant, 1KHz of 3.2 - 10.2 [-]

ASTM D150

Dielectric strength

23.0 °C

51.2 - 59.1 kV/mm

Show Supplier Material materials with Dielectric strength of 51.2 - 59.1 kV/mm

ASTM D149

Dissipation factor, 100kHz

23.0 °C

0.02 - 0.19 [-]

Show Supplier Material materials with Dissipation factor, 100kHz of 0.02 - 0.19 [-]

ASTM D150

Surface resistivity

23.0 °C

5.30E+11 - 5.50E+11 Ω/sq

Show Supplier Material materials with Surface resistivity of 5.30E+11 - 5.50E+11 Ω/sq

ASTM D257

Optical

PropertyValueComment

Refractive index

1.41 [-]

Show Supplier Material materials with Refractive index of 1.41 [-]

ASTM D542, sodium D line

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

2.5 - 7.5 g/10min

Show Supplier Material materials with Melt mass-flow rate of 2.5 - 7.5 g/10min

ASTM D1238, 230°C/12.5kg

Melt viscosity

23.0 °C

2000 - 2600 Pa·s

Show Supplier Material materials with Melt viscosity of 2000 - 2600 Pa·s

ASTM D3835

Technological properties

Property
Application areas

Fluoropolymer Processing Aids,Automotive Cables,Performance Wire,Plenum Cable

Processing methods

Compression Molding:

  • Molding temperature (°C) ISO 293: 225
  • Molding time (min) ISO 293: 3
  • DeMolding temperature (°C) ISO 293: 120