Kynar Flex® LBG2200LX America

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® LBG2200LX is a lithium ion battery grade latex of vinylidene fluoride and hexafluoropropylene designed for high performance.

Main Characteristics:

  • Same backbone as the well-known Kynar Flex® LBG grade
  • High solid content
  • Very stable latex

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Thermal

    PropertyValueComment

    Melting point

    148 - 154 °C

    Show Supplier Material materials with Melting point of 148 - 154 °C

    ASTM D3418

    Rheological Properties

    PropertyTemperatureValueComment

    Melt viscosity

    23.0 °C

    3200 - 3700 Pa·s

    Show Supplier Material materials with Melt viscosity of 3200 - 3700 Pa·s

    ASTM D3835

    Technological properties

    Property
    Application areas

    Lithium Ion Battery Binder,Lithium ion Battery Separator Coating