Kynar Flex® LBG8200 America

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® LBG8200 is a copolymer of vinylidene fluoride and hexafluoropropylene specifically designed to bring a high level of adhesion between the separator and the battery electrodes.

Main Characteristics:

  • High adhesion
  • Fast dissolution in typical solvents
  • High molecular weight

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    1.78 g/cm³

    Show Supplier Material materials with Density of 1.78 g/cm³

    min., ASTM D792

    Thermal

    PropertyValueComment

    Melting point

    142 - 148 °C

    Show Supplier Material materials with Melting point of 142 - 148 °C

    ASTM D3418

    Rheological Properties

    PropertyTemperatureValueComment

    Melt viscosity

    23.0 °C

    6800 - 7800 Pa·s

    Show Supplier Material materials with Melt viscosity of 6800 - 7800 Pa·s

    ASTM D3835

    Technological properties

    Property
    Application areas

    Lithium Ion Battery Binder,Lithium ion Battery Separator Coating