Kynar® 1000 HD America

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar® resins are fluorinated thermoplastic homopolymers.

Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo mechanical properties.

Kynar® 1000 HD resin is a standard grade of granules for compression and transfer molding, for extrusion of thick walled parts: blocks, rods, plaques, tubes.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.77 - 1.79 g/cm³

Show Supplier Material materials with Density of 1.77 - 1.79 g/cm³

ASTM D792

Limiting oxygen index

23.0 °C

60 %

Show Supplier Material materials with Limiting oxygen index of 60 %

ASTM D2863

Water absorption

23.0 °C

0.01 - 0.03 %

Show Supplier Material materials with Water absorption of 0.01 - 0.03 %

ASTM D570

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

68.9 - 103 MPa

Show Supplier Material materials with Compressive strength of 68.9 - 103 MPa

ASTM D695

Elongation

23.0 °C

20 - 100 %

Show Supplier Material materials with Elongation of 20 - 100 %

ASTM D638

Flexural modulus

23.0 °C

1.45 - 2.31 GPa

Show Supplier Material materials with Flexural modulus of 1.45 - 2.31 GPa

ASTM D790

Hardness, Shore D

23.0 °C

76 - 80 [-]

Show Supplier Material materials with Hardness, Shore D of 76 - 80 [-]

ASTM D2240

Tensile strength

23.0 °C

34.5 - 55.2 MPa

Show Supplier Material materials with Tensile strength of 34.5 - 55.2 MPa

ASTM D638

Yield strength

23.0 °C

44.8 - 55.2 MPa

Show Supplier Material materials with Yield strength of 44.8 - 55.2 MPa

ASTM D638

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.19E-4 - 1.44E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.19E-4 - 1.44E-4 1/K

ASTM D696

Glass transition temperature

-40 °C

Show Supplier Material materials with Glass transition temperature of -40 °C

ASTM D7028

Heat deflection temperature, 0.45 MPa

125 - 140 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 125 - 140 °C

ASTM D648, 248 °F/hr

Heat deflection temperature, 1.80 MPa

105 - 115 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 105 - 115 °C

ASTM D648, 248 °F/hr

Melting point

172 °C

Show Supplier Material materials with Melting point of 172 °C

ASTM D3418

Relative temperature index, electrical

150 °C

Show Supplier Material materials with Relative temperature index, electrical of 150 °C

UL 746B

Relative temperature index, mechanical strength

150 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C

UL 746B

Specific heat capacity

23.0 °C

745 - 958 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 745 - 958 J/(kg·K)

DSC

Thermal conductivity

23.0 °C

0.17 - 0.19 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.17 - 0.19 W/(m·K)

ASTM D433

Thermal decomposition in air

375 °C

Show Supplier Material materials with Thermal decomposition in air of 375 °C

TGA, 1% wt. loss

Thermal decomposition in nitrogen

410 °C

Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C

TGA, 1% wt. loss

Flammability

At thickness 1.6 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0

Electrical

PropertyTemperatureValueComment

Volume resistivity

23.0 °C

2.00E+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 2.00E+14 Ω·cm

ASTM D257, 65% RH

Optical

PropertyValueComment

Refractive index

1.42 [-]

Show Supplier Material materials with Refractive index of 1.42 [-]

ASTM D542, sodium D line

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

1 - 3 g/10min

Show Supplier Material materials with Melt mass-flow rate of 1 - 3 g/10min

ASTM D1238, 230°C/5kg

Melt viscosity

23.0 °C

1500 - 2000 Pa·s

Show Supplier Material materials with Melt viscosity of 1500 - 2000 Pa·s

ASTM D3835

Technological properties

Property
Application areas

Chemical Process Industry,Chemical Process Industry - High Purity Piping,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes,Plenum Pipe,Tubing and Hoses