Alternative and trade names
PVDF-CD
Want to keep this datasheet? Save it now in your required format

Description

Kynar® resins are fluorinated thermoplastic homopolymers.

Kynar® 340 resin is a thermoplastic fluorinated polymer resin. The properties are the same as standard grade: chemical resistance, resistance to UV, low permeation, high purity, excellent mechanical behavior. More over, this grade is electrically conductive. This grade is available as pellet form for injection, extrusion, compression.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.84 - 1.88 g/cm³

Show Supplier Material materials with Density of 1.84 - 1.88 g/cm³

ASTM D792

Thermal

PropertyValueComment

Melting point

165 - 172 °C

Show Supplier Material materials with Melting point of 165 - 172 °C

ASTM D3418

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

3 - 8 g/10min

Show Supplier Material materials with Melt mass-flow rate of 3 - 8 g/10min

ASTM D1238, 230°C/10kg

Melt viscosity

23.0 °C

2500 Pa·s

Show Supplier Material materials with Melt viscosity of 2500 Pa·s

ASTM D3835

Technological properties

Property
Application areas

Fuel Management - In-Tank and Fuel Venting Lines,Chemical Process Industry,Chemical Process Industry - Stock Shapes,Permanent Antistatic Solutions

Fillers

Carbon Black