The material: 'Kynar® 460' you were looking for has been superseded by the one below.

Kynar® 460

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar® resins are fluorinated thermoplastic homopolymers.

Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo-mechanical properties.

Kynar® 460 resin is a standard grade of granules for extrusion of tubes, cables and plaques, compression and transfer molding.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTesting StandardConditionComment

Coefficient of friction

0.17 [-]

Show Supplier Material materials with Coefficient of friction of 0.17 [-]

ASTM D1894

vs Steel, Kinetic

0.23 [-]

Show Supplier Material materials with Coefficient of friction of 0.23 [-]

ASTM D1894

vs Steel, Static

Density

1.75 - 1.77 g/cm³

Show Supplier Material materials with Density of 1.75 - 1.77 g/cm³

ASTM D792

1.76 g/cm³

Show Supplier Material materials with Density of 1.76 g/cm³

ISO 1183

dry

Limiting oxygen index

43 %

Show Supplier Material materials with Limiting oxygen index of 43 %

ISO 4589-1/-2

dry

44 %

Show Supplier Material materials with Limiting oxygen index of 44 %

ASTM D2863

Water absorption

0.04 %

Show Supplier Material materials with Water absorption of 0.04 %

Sim. to ISO 62, ASTM D570

max.

Mechanical

PropertyTemperatureValueTesting StandardConditionComment

Compressive strength

55.2 - 68.9 MPa

Show Supplier Material materials with Compressive strength of 55.2 - 68.9 MPa

ASTM D695

Elastic modulus

1.0 - 1.4 GPa

Show Supplier Material materials with Elastic modulus of 1.0 - 1.4 GPa

ASTM D638

1.4 GPa

Show Supplier Material materials with Elastic modulus of 1.4 GPa

ISO 527-1/-2

dry

Elongation

50 - 250 %

Show Supplier Material materials with Elongation of 50 - 250 %

ASTM D638

50 %

Show Supplier Material materials with Elongation of 50 %

ISO 527-1/-2

dry

min. | nominal

Elongation at yield

10 - 15 %

Show Supplier Material materials with Elongation at yield of 10 - 15 %

ASTM D638

13 %

Show Supplier Material materials with Elongation at yield of 13 %

ISO 527-1/-2

dry

Flexural modulus

1.4 - 1.8 GPa

Show Supplier Material materials with Flexural modulus of 1.4 - 1.8 GPa

ASTM D790

Flexural strength

48.3 - 62.1 MPa

Show Supplier Material materials with Flexural strength of 48.3 - 62.1 MPa

ASTM D790

at 5% strain

Hardness, Shore D

75 - 80 [-]

Show Supplier Material materials with Hardness, Shore D of 75 - 80 [-]

ASTM D2240

Impact strength, Charpy notched, ASTM

23 °C

96.1 - 214 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 96.1 - 214 J/m

ASTM D256

Impact strength, Charpy unnotched, ASTM

23 °C

801 - 2140 J/m

Show Supplier Material materials with Impact strength, Charpy unnotched, ASTM of 801 - 2140 J/m

ASTM D256

Tensile strength

31 - 48.3 MPa

Show Supplier Material materials with Tensile strength of 31 - 48.3 MPa

ASTM D638

Yield strength

34.5 - 51.7 MPa

Show Supplier Material materials with Yield strength of 34.5 - 51.7 MPa

ASTM D638

52 MPa

Show Supplier Material materials with Yield strength of 52 MPa

ISO 527-1/-2

dry

Thermal

PropertyValueTesting StandardConditionPressureComment

Coefficient of thermal expansion

9e-05 - 0.000126 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9e-05 - 0.000126 1/K

ASTM D696

Glass transition temperature

-40.6 - -38.3 °C

Show Supplier Material materials with Glass transition temperature of -40.6 - -38.3 °C

ASTM D7028

-40 °C

Show Supplier Material materials with Glass transition temperature of -40 °C

ISO 11357-1/-2

dry

10°C/min

Heat deflection temperature

80 - 90 °C

Show Supplier Material materials with Heat deflection temperature of 80 - 90 °C

ASTM D648

2 MPa

248 °F/hr

85 °C

Show Supplier Material materials with Heat deflection temperature of 85 °C

ISO 75-1/-2

dry

2 MPa

112 - 140 °C

Show Supplier Material materials with Heat deflection temperature of 112 - 140 °C

ASTM D648

0.45 MPa

248 °F/hr

Melting point

155 - 172 °C

Show Supplier Material materials with Melting point of 155 - 172 °C

ASTM D3418

161 °C

Show Supplier Material materials with Melting point of 161 °C

ISO 11357-1/-3

dry

10°C/min

Specific heat capacity

745 - 958 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 745 - 958 J/(kg·K)

DSC

Thermal conductivity

0.17 - 0.19 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.17 - 0.19 W/(m·K)

ASTM D433

Thermal decomposition in air

375 °C

Show Supplier Material materials with Thermal decomposition in air of 375 °C

TGA

1% wt. loss

Thermal decomposition in nitrogen

410 °C

Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C

TGA

1% wt. loss

Flammability

At thickness 1.6 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0

Electrical

PropertyValueFrequencyTesting StandardCondition

Dielectric constant

4.5 - 9.5 [-]

Show Supplier Material materials with Dielectric constant of 4.5 - 9.5 [-]

1KHz

ASTM D150

6.7 [-]

Show Supplier Material materials with Dielectric constant of 6.7 [-]

1MHz

IEC 60250

dry

9 [-]

Show Supplier Material materials with Dielectric constant of 9 [-]

100Hz

IEC 60250

dry

Dielectric strength

63 kV/mm

Show Supplier Material materials with Dielectric strength of 63 kV/mm

ASTM D149, IEC 60243-1

dry

Dissipation factor

0.01 - 0.21 [-]

Show Supplier Material materials with Dissipation factor of 0.01 - 0.21 [-]

100KHz

ASTM D150

0.07 [-]

Show Supplier Material materials with Dissipation factor of 0.07 [-]

1MHz

IEC 60250

dry

0.13 [-]

Show Supplier Material materials with Dissipation factor of 0.13 [-]

100Hz

IEC 60250

dry

Surface resistivity

5.1e+11 - 5.3e+11 Ω/sq

Show Supplier Material materials with Surface resistivity of 5.1e+11 - 5.3e+11 Ω/sq

ASTM D257

Volume resistivity

2e+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm

ASTM D257

65% RH

2e+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm

IEC 60093

dry

Optical

PropertyValueTesting StandardComment

Refractive index

1 [-]

Show Supplier Material materials with Refractive index of 1 [-]

ASTM D542

sodium D line

Rheological Properties

PropertyValueTesting StandardConditionComment

Melt mass-flow rate

6 - 14 g/10min

Show Supplier Material materials with Melt mass-flow rate of 6 - 14 g/10min

ASTM D1238

230°C/21.6kg

Melt viscosity

2350 - 2950 Pa·s

Show Supplier Material materials with Melt viscosity of 2350 - 2950 Pa·s

ASTM D3835

Melt volume-flow rate

5.6 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 5.6 cm³/10min

ISO 1133

dry

230°C/21.6kg

Shrinkage

2 %

Show Supplier Material materials with Shrinkage of 2 %

ISO 294-4

dry

2 %

Show Supplier Material materials with Shrinkage of 2 %

ISO 294-4

dry

Transverse

Thermal conductivity of melt

0.19 W/(m·K)

Show Supplier Material materials with Thermal conductivity of melt of 0.19 W/(m·K)

Technological properties

Property
Application areas

Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes,Monofilaments,Tower Packing,Automotive Cables,Performance Wire,Plenum Cable,PVDF Cable Jacketing,Wire and Cables