Description

Kynar® resins are fluorinated thermoplastic homopolymers. This product is used for the co-extrusion of Rilsan® polyamides and Kynar® PVDF resins for the preparation of multilayer tubing or film.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

100 %

Show Supplier Material materials with Elongation of 100 %

min., ASTM D638

Thermal

PropertyValueComment

Melting point

166 °C

Show Supplier Material materials with Melting point of 166 °C

ASTM D3418

Rheological Properties

PropertyTemperatureValueComment

Melt viscosity

23.0 °C

160 Pa·s

Show Supplier Material materials with Melt viscosity of 160 Pa·s

ASTM D3835

Technological properties

Property
Application areas

Fuel Management - Fuel Lines