General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.78 g/cm³ Show Supplier Material materials with Density of 1.78 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | min. | nominal |
Elongation at yield | 8 % Show Supplier Material materials with Elongation at yield of 8 % | dry | ISO 527-1/-2 | |
Yield strength | 30 MPa Show Supplier Material materials with Yield strength of 30 MPa | dry | ISO 527-3 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Heat deflection temperature | 108 °C Show Supplier Material materials with Heat deflection temperature of 108 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
Melting point | 170 °C Show Supplier Material materials with Melting point of 170 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Flammability | At thickness 0.8 mm IEC 60695-11-10: HB |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melt volume-flow rate | 15 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 15 cm³/10min | dry | ISO 1133 | 230°C/3.8kg |
Technological properties
Property | ||
---|---|---|
Application areas | Underground Fuel Containment |