Kynar® HSV 1800

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar® resins are fluorinated thermoplastic polymers, specially designed to bring a high level of adhesion even at a very low binder content. This binder can be used for cathode and anode formulation.

Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo mechanical properties.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueConditionTesting Standard

Density

1.78 g/cm³

Show Supplier Material materials with Density of 1.78 g/cm³

dry

ISO 1183

Technological properties

Property
Application areas

Lithium Ion Battery Binder