The material: 'Polyamide Nylon 6 Film' you were looking for has been superseded by the one below.

Orgalloy® R60 ES NAT

Alternative and trade names
PA6
Want to keep this datasheet? Save it now in your required format

Description

Orgalloy® R 60 ES NAT resin is a polyamide alloy especially designed for blown film extrusion. This natural grade dedicated to extrusion offers good barrier properties and chemical resistance to solvents and alcohols while exhibiting a low surface tension (easy release).

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.03 g/cm³

Show Supplier Material materials with Density of 1.03 g/cm³

dry

ISO 1183

Moisture absorption

1.3 %

Show Supplier Material materials with Moisture absorption of 1.3 %

Sim. to ISO 62

Water absorption

3.3 %

Show Supplier Material materials with Water absorption of 3.3 %

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

1.9 GPa

Show Supplier Material materials with Elastic modulus of 1.9 GPa

cond.

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

cond.

ISO 527-1/-2

min. | nominal

530 %

Show Supplier Material materials with Elongation of 530 %

dry

ISO 527-3

Transverse

530 %

Show Supplier Material materials with Elongation of 530 %

dry

ISO 527-3

Elongation at yield

3.4 %

Show Supplier Material materials with Elongation at yield of 3.4 %

cond.

ISO 527-1/-2

20 %

Show Supplier Material materials with Elongation at yield of 20 %

dry

ISO 527-3

Elongation at yield, transverse

15 %

Show Supplier Material materials with Elongation at yield, transverse of 15 %

dry

ISO 527-3

Hardness, Shore D

73 [-]

Show Supplier Material materials with Hardness, Shore D of 73 [-]

dry

ISO 7619-1

15 seconds

Impact strength, Charpy notched

23 °C

9 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m²

cond.

ISO 179/1eA

Impact strength, Charpy unnotched

No Break at 23°C

cond.

ISO 179/1eU

Tear force

35 N

Show Supplier Material materials with Tear force of 35 N

ISO 6383-2

Transverse

40 N

Show Supplier Material materials with Tear force of 40 N

ISO 6383-2

Tensile strength

60 MPa

Show Supplier Material materials with Tensile strength of 60 MPa

dry

ISO 527-3

Transverse

80 MPa

Show Supplier Material materials with Tensile strength of 80 MPa

dry

ISO 527-3

Yield strength

33 MPa

Show Supplier Material materials with Yield strength of 33 MPa

dry

ISO 527-3

Transverse

47 MPa

Show Supplier Material materials with Yield strength of 47 MPa

cond.

ISO 527-1/-2

55 MPa

Show Supplier Material materials with Yield strength of 55 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardPressureComment

Coefficient of thermal expansion

9.3e-05 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9.3e-05 1/K

dry

ISO 11359-1/-2

0.000133 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.000133 1/K

dry

ISO 11359-1/-2

Transverse

Heat deflection temperature

75 °C

Show Supplier Material materials with Heat deflection temperature of 75 °C

dry

ISO 75-1/-2

2 MPa

130 °C

Show Supplier Material materials with Heat deflection temperature of 130 °C

dry

ISO 75-1/-2

0.45 MPa

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

dry

ISO 11357-1/-3

10°C/min

Vicat softening temperature

134 °C

Show Supplier Material materials with Vicat softening temperature of 134 °C

ISO 306

50°C/h 50N

Flammability

At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: HB

Electrical

PropertyValueConditionTesting StandardFrequencyComment

Comparative tracking index

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

cond.

IEC 60112

Dielectric constant

3 [-]

Show Supplier Material materials with Dielectric constant of 3 [-]

cond.

IEC 60250

100Hz

3 [-]

Show Supplier Material materials with Dielectric constant of 3 [-]

IEC 60250

1MHz

Dielectric strength

38 kV/mm

Show Supplier Material materials with Dielectric strength of 38 kV/mm

cond., dry

IEC 60243-1

Dissipation factor

0.025 [-]

Show Supplier Material materials with Dissipation factor of 0.025 [-]

cond.

IEC 60250

1MHz

0.062 [-]

Show Supplier Material materials with Dissipation factor of 0.062 [-]

cond.

IEC 60250

100Hz

Surface resistivity

1e+15 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq

cond.

IEC 60093

min.

Volume resistivity

1e+13 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm

cond.

IEC 60093

min.

Rheological Properties

PropertyValueConditionTesting StandardComment

Melt volume-flow rate

2.5 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 2.5 cm³/10min

dry

ISO 1133

235°C/2.16kg

Technological properties

Property
Application areas

Mold Release Film

Processing methods

Injection Molding:

  • Melt temperature (°C) ISO 294: 260
  • Mold temperature (°C) ISO 10724: 60
  • Injection velocity (mm/s) ISO 294: -
  • Pressure at hold (MPa) ISO 294: -

  • Film Extrusion:

  • Drying time (only necessary for bags opened for more than two hours): 4-8 hours at 80°C
  • Extrusion melt temperature (min-recommended-max): 250-260-270°C