Platamid® M 1657

Alternative and trade names
PA*
Want to keep this datasheet? Save it now in your required format

Description

Platamid® M 1657

Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® M 1657 is a standard thermoplastic co-polyamide hot melt adhesive available in pellet form. This very low melt viscosity, fast re-crystallizing grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments.

Platamid® M 1657 offers a very good adhesion to various polar substrates (thermoplastics, thermosets, metal natural fibers, etc).

Platamid® M 1657 has a very good dry cleaning resistance and washing resistance up to 40°C.

This product is available:

  • Dried with optical brightener (M 1657 TA)
  • Un-dried with optical brightener (M 1657 FA)

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    1.07 g/cm³

    Show Supplier Material materials with Density of 1.07 g/cm³

    ISO 1183

    Thermal

    PropertyValueComment

    Melting point

    107 °C

    Show Supplier Material materials with Melting point of 107 °C

    ISO 11357-1/-3, 10°C/min

    Rheological Properties

    PropertyValueComment

    Melt volume-flow rate

    200 cm³/10min

    Show Supplier Material materials with Melt volume-flow rate of 200 cm³/10min

    ISO 1133, 160°C/2.16kg

    Technological properties

    Property
    Application areas

    Accessories

    Other

    PACKAGING

    Platamid® M 1657 TA is delivered in 25 kg sealed bags. Platamid®M 1657 FA is delivered in 25 kg sealed bags and 500 kg sealed big bags (GRVS). These grades are ready to be processed.

    SHELF LIFE

    Two years from the date of delivery. For any use above this limit, please refer to our technical services.