Rilsan® MINICOAT WHITE 1452 MAC resin

  • Rilsan® POLYAMIDE 11 (PA11) powder

    Melt mix white powder for coating of small metallic parts using Arkema's Minicoat process. The range includes several colors. The properties listed in the data base have been measured on a corresponding Rilsan® PA11 granule.

  • This material data has been provided by Arkema Technical Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValueConditionTesting Standard

    Density

    1.1 g/cm³

    Show Supplier Material materials with Density of 1.1 g/cm³

    dry

    ISO 1183

    Water absorption

    1.9 %

    Show Supplier Material materials with Water absorption of 1.9 %

    Sim. to ISO 62

    Thermal

    PropertyValueConditionTesting StandardComment

    Melting point

    185 °C

    Show Supplier Material materials with Melting point of 185 °C

    dry

    ISO 11357-1/-3

    10°C/min

    Vicat softening temperature

    160 °C

    Show Supplier Material materials with Vicat softening temperature of 160 °C

    ISO 306

    50°C/h 50N

    Flammability

    At thickness 1.6 mm IEC 60695-11-10: V-2, At thickness 3.2 IEC 60695-11-10: V-2

    Electrical

    PropertyValueConditionTesting Standard

    Dielectric strength

    30 kV/mm

    Show Supplier Material materials with Dielectric strength of 30 kV/mm

    dry

    IEC 60243-1

    Surface resistivity

    1e+14 Ω/sq

    Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq

    cond.

    IEC 60093

    Volume resistivity

    1e+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm

    dry

    IEC 60093

    Technological properties

    Property
    Application areas

    Powder Coatings - Automotive & Transportation,Powder Coatings - Exterior Applications,Powder Coatings - General Purpose,Powder Coatings - Undergarments,Powder Coatings - Wire Goods

    Color

    White