General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 1.5 - 1.54 g/cm³ Show Supplier Material materials with Density of 1.5 - 1.54 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 13 - 14 GPa Show Supplier Material materials with Elastic modulus of 13 - 14 GPa | ISO 527-2 |
Elongation | 20.0 °C | 2.2 - 2.8 % Show Supplier Material materials with Elongation of 2.2 - 2.8 % | ISO 527-1/-2 |
Impact strength, Charpy notched | 20.0 °C | 10 - 14 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 - 14 kJ/m² | ISO 179/1eA |
Impact strength, Charpy unnotched | 20.0 °C | 60 - 80 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 60 - 80 kJ/m² | ISO 179/1eA |
Tensile strength | 20.0 °C | 165 - 185 MPa Show Supplier Material materials with Tensile strength of 165 - 185 MPa | ISO 527-1/-2 |
Thermal
Property | Temperature | Value |
---|---|---|
Ash content | 20.0 °C | 47 - 53 % Show Supplier Material materials with Ash content of 47 - 53 % |
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt volume-flow rate | 10 - 50 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 10 - 50 cm³/10min | ISO 1133, 275°C/5Kg |
Technological properties
Property | ||
---|---|---|
Application areas | Cable protection parts for vehicles, Cable ties, Electrical and electronic application, Acoustic components, Cable ducts, brackets in the automotive sector, covers, frames, Reinforcing elements, Radiator cowl, Gear lever housing, Fans / Frames, Parts for furniture and chair industry | |
Fillers | 50% Glass Fiber | |
Processing methods | Pre-drying 2-4 hours/80°C |