Dimension
Property | Value |
---|---|
Thickness | 5 mm Show Supplier Material materials with Thickness of 5 mm |
Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 8 % Show Supplier Material materials with Elongation of 8 % |
Elongation A50 | 23.0 °C | 6 % Show Supplier Material materials with Elongation A50 of 6 % |
Hardness, Brinell | 23.0 °C | 95 [-] Show Supplier Material materials with Hardness, Brinell of 95 [-] |
Tensile strength | 23.0 °C | 290 MPa Show Supplier Material materials with Tensile strength of 290 MPa |
Yield strength Rp0.2 | 23.0 °C | 250 MPa Show Supplier Material materials with Yield strength Rp0.2 of 250 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | balance |
Chromium | 0.25 % Show Supplier Material materials with Chromium of 0.25 % |
Copper | 0.1 % Show Supplier Material materials with Copper of 0.1 % |
Iron | 0.5 % Show Supplier Material materials with Iron of 0.5 % |
Magnesium | 0.6 - 1.2 % Show Supplier Material materials with Magnesium of 0.6 - 1.2 % |
Manganese | 0.4 - 1 % Show Supplier Material materials with Manganese of 0.4 - 1 % |
Other | 0.05 - 0.15 % Show Supplier Material materials with Other of 0.05 - 0.15 % |
Silicon | 0.7 - 1.3 % Show Supplier Material materials with Silicon of 0.7 - 1.3 % |
Titanium | 0.1 % Show Supplier Material materials with Titanium of 0.1 % |
Zinc | 0.2 % Show Supplier Material materials with Zinc of 0.2 % |