EN AW-6063 T64

Alternative and trade names
DIN AlMg0.7Si
Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Braz Line.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Thickness

15 mm

Show Supplier Material materials with Thickness of 15 mm

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

12 %

Show Supplier Material materials with Elongation of 12 %

Elongation A50

23.0 °C

10 %

Show Supplier Material materials with Elongation A50 of 10 %

Hardness, Brinell

23.0 °C

65 [-]

Show Supplier Material materials with Hardness, Brinell of 65 [-]

Tensile strength

23.0 °C

180 MPa

Show Supplier Material materials with Tensile strength of 180 MPa

Yield strength Rp0.2

23.0 °C

120 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 120 MPa

Chemical properties

PropertyValue

Aluminium

balance

Chromium

0.1 %

Show Supplier Material materials with Chromium of 0.1 %

Copper

0.1 %

Show Supplier Material materials with Copper of 0.1 %

Iron

0.35 %

Show Supplier Material materials with Iron of 0.35 %

Magnesium

0.45 - 0.9 %

Show Supplier Material materials with Magnesium of 0.45 - 0.9 %

Manganese

0.1 %

Show Supplier Material materials with Manganese of 0.1 %

Other

0.05 - 0.15 %

Show Supplier Material materials with Other of 0.05 - 0.15 %

Silicon

0.2 - 0.6 %

Show Supplier Material materials with Silicon of 0.2 - 0.6 %

Titanium

0.1 %

Show Supplier Material materials with Titanium of 0.1 %

Zinc

0.1 %