EN AW-1050A F

Alternative and trade names
DIN Al99.5
Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Braz Line.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

25 %

Show Supplier Material materials with Elongation of 25 %

Elongation A50

23.0 °C

23 %

Show Supplier Material materials with Elongation A50 of 23 %

Hardness, Brinell

23.0 °C

20 [-]

Show Supplier Material materials with Hardness, Brinell of 20 [-]

Tensile strength

23.0 °C

60 MPa

Show Supplier Material materials with Tensile strength of 60 MPa

Yield strength Rp0.2

23.0 °C

20 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 20 MPa

Chemical properties

PropertyValue

Aluminium

99.5 %

Show Supplier Material materials with Aluminium of 99.5 %

Copper

0.05 %

Show Supplier Material materials with Copper of 0.05 %

Iron

0.4 %

Show Supplier Material materials with Iron of 0.4 %

Magnesium

0.05 %

Show Supplier Material materials with Magnesium of 0.05 %

Manganese

0.05 %

Show Supplier Material materials with Manganese of 0.05 %

Other

0.03 %

Show Supplier Material materials with Other of 0.03 %

Silicon

0.25 %

Show Supplier Material materials with Silicon of 0.25 %

Titanium

0.05 %

Show Supplier Material materials with Titanium of 0.05 %

Zinc

0.07 %

Show Supplier Material materials with Zinc of 0.07 %

Technological properties

Property
Coating

suitable for electro-chemical brightening and anodizing

Corrosion properties

corrosion resistant

Processing methods

Excellent forming properties

Welding

weldable