Customize your search with filters
Material Supplied by
The CTCK110 grade is Ceratizit's high-performance grade for cast iron machining. This extremely wear-resistant grade for the K10 ISO application range is used when cast iron is machined at high cutting parameters. The prerequisites for this type of machining are a continuous cut and a stable machining situation.
Grain structure
Fine grain size (of hard metal base material)
Layer system
CVD / Ti(CN) + Al₂O₃
Flexural strength σbend
2900 MPa at 20 °C
DIN EN ISO 7438 (of hard metal base material)
Fracture toughness KIC
9 MPa·√m at 20 °C
of hard metal base material
Hardness, Vickers, 30 HV 30
1810 [-] at 20 °C
of hard metal base material
Element
Weight %
Comment
-
WC balance
5 %
2 %
as mixed carbide
Application areas
The first choice for the machining of cast iron at high cutting speeds with continuous cut.
Coating
CVD coated
This material data has been provided by Ceratizit.