CTPM240 (PVD coated carbide)

.XLSX
.PDF
Save

Description

Primary standard name

Equivalent standard names

Properties

General

Grain size dgrain

1 μm

of hard metal base material

Layer system

PVD; TiAlTaN

Layer thickness t

5 µm

Mechanical

Flexural strength σbend

3500 MPa at 20 °C

DIN EN ISO 7438 (of hard metal base material)

Fracture toughness KIC

12 MPa·√m at 20 °C

of hard metal base material

Hardness, Vickers, 30 HV 30

1380 [-] at 20 °C

of hard metal base material

Chemical properties

Element

Weight %

Comment

W

-

WC balance

Co

12.5 %

C

2 %

as mixed carbide

Technological properties

Application areas

The first choice for the machining of austenitic steels.

Coating

PVD coated

This material data has been provided by Ceratizit.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.