Bismuth sodium barium titanate ((1-x)BNT-xBT) Powder

Alternative and trade names
BNT-BT, BNT-6Ba, NBT-6BT, NBT-6Ba, BNBT, Bismuth sodium barium titanate
Want to keep this datasheet? Save it now in your required format

Description

(1-x)BNT-xBT is supplied as fine, white submicron powder with a chemical purity > 99% (Phase pure by XRD).

This material data has been provided by Cerpotech.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Bulk density

23.0 °C

5.97 g/cm³

Show Supplier Material materials with Bulk density of 5.97 g/cm³

Technological properties

Property
Application areas

energy harvesting, lead-free piezoelectric, actuator, electro caloric cooling device, high strain application, energy storage, transducer, sensor

Chemical composition

Bi0.47Na0.47Ba0.06TiO3

Color

Fine, white powder

Crystal structure

Crystal structure at 25°C: Pseudocubic/R3c

Processing history

Cerpotech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, Cerpotech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices.