NN is supplied as fine, white submicron powder with a chemical purity > 99% (Phase pure by XRD).
Particle size d
BET
Chemical composition
NANbO3
Color
Fine, white powder
Processing history
CerPoTech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, CerPoTech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices.