General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.75 g/cm³ Show Material materials with Density of 8.75 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 135 GPa Show Material materials with Elastic modulus of 135 GPa |
Elongation | 23.0 °C | 45 % Show Material materials with Elongation of 45 % |
Hardness, Vickers | 23.0 °C | 80 [-] Show Material materials with Hardness, Vickers of 80 [-] |
Tensile strength | 23.0 °C | 390 MPa Show Material materials with Tensile strength of 390 MPa |
Yield strength Rp0.2 | 23.0 °C | 120 MPa Show Material materials with Yield strength Rp0.2 of 120 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Melting point | 1060 - 1110 °C Show Material materials with Melting point of 1060 - 1110 °C | |
Thermal conductivity | 23.0 °C | 25 W/(m·K) Show Material materials with Thermal conductivity of 25 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 3.48E+6 S/m Show Material materials with Electrical conductivity of 3.48E+6 S/m |
Electrical resistivity | 23.0 °C | 2.9E-7 Ω·m Show Material materials with Electrical resistivity of 2.9E-7 Ω·m |
Specific Electrical conductivity | 6 % IACS Show Material materials with Specific Electrical conductivity of 6 % IACS |
Magnetic
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetic permeability | 23.0 °C | 1.05 [-] Show Material materials with Relative magnetic permeability of 1.05 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Copper | 60 - 65 % Show Material materials with Copper of 60 - 65 % | ||
Iron | 0.3 % Show Material materials with Iron of 0.3 % | max. | |
Lead | 0.03 % Show Material materials with Lead of 0.03 % | max. | |
Manganese | 0.05 - 0.5 % Show Material materials with Manganese of 0.05 - 0.5 % | ||
Nickel | 17 - 19 % Show Material materials with Nickel of 17 - 19 % | ||
Zinc | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | General: Architectural metalwork, panels and trim, holloware, musical instruments, medals and medallions, costume jewellery, nameplates, cosmetic cases, lamp caps, lighting fittings, platters, bowls, dials, relay and contact springs, medical, industrial and scientific instrument components | |
Cold Forming | Very good cold working characteristics | |
Corrosion properties | Excellent corrosion resistance |