The material: 'SILVERSPEED-XL Nickel Silver' you were looking for has been superseded by the one below.

SILVERSPEED-XL Nickel Silver

Want to keep this datasheet? Save it now in your required format

Description

SILVERSPEED-XL is a copper alloy with additions of zinc and nickel to give an attractive soft silvery colour not as brash as stainless steel. It is a truly superlative free-machining alloy with a machinability rating almost the same as free cutting brass. It is highly recommended for the production of intricate components by complex machining operations. This grade is stocked exclusively by Columbia Metals and has the same application and performance characteristics as NS101. However, the invaluable increase of around 20% in machinability over NS101 can provide clean, burr free, close tolerance, high surface quality components at maximum production speeds and prolonged tool life. SILVERSPEED-XL is a copper alloy with additions of zinc and nickel to give an attractive soft silvery colour not as brash as stainless steel. It is a truly superlative free-machining aloy with a machinability rating almost the same as free cutting brass. It is highly recommended for the production of intricate components by complex machining operations. This grade is stocked exclusively by Columbia Metals and has the same application and performance characteristics as NS101. However, the invaluable increase of around 20% in machinability over NS101 can provide clean, burr free, close tolerance, high surface quality components at maximum production speeds and prolonged tool life.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.44 g/cm³

Show Material materials with Density of 8.44 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

120 GPa

Show Material materials with Elastic modulus of 120 GPa

Elongation

23.0 °C

20 %

Show Material materials with Elongation of 20 %

Hardness, Vickers

23.0 °C

185 [-]

Show Material materials with Hardness, Vickers of 185 [-]

Tensile strength

23.0 °C

560 MPa

Show Material materials with Tensile strength of 560 MPa

Yield strength Rp0.2

23.0 °C

450 MPa

Show Material materials with Yield strength Rp0.2 of 450 MPa

Thermal

PropertyTemperatureValue

Melting point

850 - 870 °C

Show Material materials with Melting point of 850 - 870 °C

Thermal conductivity

23.0 °C

30 W/(m·K)

Show Material materials with Thermal conductivity of 30 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

2.90E+6 S/m

Show Material materials with Electrical conductivity of 2.90E+6 S/m

Electrical resistivity

23.0 °C

3.4E-7 Ω·m

Show Material materials with Electrical resistivity of 3.4E-7 Ω·m

Specific Electrical conductivity

5 % IACS

Show Material materials with Specific Electrical conductivity of 5 % IACS

Magnetic

PropertyTemperatureValueComment

Relative magnetic permeability

23.0 °C

1.05 [-]

Show Material materials with Relative magnetic permeability of 1.05 [-]

max.

Chemical properties

PropertyValueComment

Copper

47 - 50 %

Show Material materials with Copper of 47 - 50 %

Iron

0.3 %

Show Material materials with Iron of 0.3 %

max.

Lead

2.3 - 3.3 %

Show Material materials with Lead of 2.3 - 3.3 %

Manganese

1.5 - 3 %

Show Material materials with Manganese of 1.5 - 3 %

Nickel

6 - 8 %

Show Material materials with Nickel of 6 - 8 %

Zinc

Balance

Technological properties

Property
Application areas

General: Gears, pinions, clock and watch parts, screws and fasteners, keys, lock parts, decorative and architectural metalwork, camera parts, electrical and electronic pins and connectors, medical, industrial and scientific instrument components

Corrosion properties

Very high corrosion resistance

General machinability

Excellent machinability