General
Property | Value | Related Standards | Shape |
---|---|---|---|
Density | 4.43 g/cm³ Show Material materials with Density of 4.43 g/cm³ | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Mechanical
Property | Value | Related Standards | Shape |
---|---|---|---|
Elastic modulus | 114.0 GPa Show Material materials with Elastic modulus of 114.0 GPa | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Elongation | 10 % Show Material materials with Elongation of 10 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Hardness, Rockwell C | 36 [-] Show Material materials with Hardness, Rockwell C of 36 [-] | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Tensile strength | 895.0 - 931.0 MPa Show Material materials with Tensile strength of 895.0 - 931.0 MPa | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Thermal
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Coefficient of thermal expansion of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | ||
Melting point | 1674 °C Show Material materials with Melting point of 1674 °C | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar | |
Specific heat capacity | 370.0 - 674.0 J/(kg·K) Show Material materials with Specific heat capacity of 370.0 - 674.0 J/(kg·K) | Typical for Titanium Alpha Beta Alloy | ||
Thermal conductivity | 6.7 W/(m·K) Show Material materials with Thermal conductivity of 6.7 W/(m·K) | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Electrical
Property | Value | Related Standards | Shape |
---|---|---|---|
Electrical resistivity | 1.8000000000000001e-06 Ω·m Show Material materials with Electrical resistivity of 1.8000000000000001e-06 Ω·m | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 5.5 - 6.75 % Show Material materials with Aluminium of 5.5 - 6.75 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Carbon | 0.1 % Show Material materials with Carbon of 0.1 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Hydrogen | 0.0125 % Show Material materials with Hydrogen of 0.0125 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Iron | 0.4 % Show Material materials with Iron of 0.4 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Nitrogen | 0.05 % Show Material materials with Nitrogen of 0.05 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Oxygen | 0.2 % Show Material materials with Oxygen of 0.2 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace: Compressor blades, discs and rings for jet engines, airframe components, fasteners, rocket engine cases, helicopter rotor blades and critical forgings;Offshore & marine: Offshore tubulars and oil and gas equipment;Other: Biomedical implants and chemical processing equipment | |
Corrosion properties | Good corrosion resistance |