Thermodur 2329 Bar

Alternative and trade names
DIN EN ISO 46CrSiMoV7, 1.2329
Want to keep this datasheet? Save it now in your required format

Description

46CrSiMoV7 (1.2329) shows the following features and properties:


  • Excellent tempering resistance
  • High-temperature strength
  • Full quenching and tempering properties
  • Outstanding weldability
  • Good machinability
  • Nitridable
  • PVD and CVD coatable
  • Equivalent Materials

    This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Dimension

    PropertyValue

    Diameter

    232 - 532 mm

    Show Supplier Material materials with Diameter of 232 - 532 mm

    Mechanical

    PropertyValueComment

    Hardness, Brinell

    230 [-]

    Show Supplier Material materials with Hardness, Brinell of 230 [-]

    soft annealed

    Hardness, Rockwell C

    46 - 52 [-]

    Show Supplier Material materials with Hardness, Rockwell C of 46 - 52 [-]

    Tensile strength

    1485 - 1775 MPa

    Show Supplier Material materials with Tensile strength of 1485 - 1775 MPa

    Chemical properties

    PropertyValue

    Carbon

    0.45 %

    Show Supplier Material materials with Carbon of 0.45 %

    Chromium

    1.8 %

    Show Supplier Material materials with Chromium of 1.8 %

    Iron

    Balance

    Manganese

    0.8 %

    Show Supplier Material materials with Manganese of 0.8 %

    Molybdenum

    0.3 %

    Show Supplier Material materials with Molybdenum of 0.3 %

    Nickel

    0.6 %

    Show Supplier Material materials with Nickel of 0.6 %

    Silicon

    0.7 %

    Show Supplier Material materials with Silicon of 0.7 %

    Vanadium

    0.2 %

    Show Supplier Material materials with Vanadium of 0.2 %

    Technological properties

    Property
    Application areas

    Forging dies, extrusion press tools, compression moulding dies

    Heat Treatment

    Soft annealing: 780-800°C (Cooling in furnace or air) - Hardening: 880-920°C and quenching in air, oil or hot bath T=500-550°C

    Welding

    Outstanding weldability