General
Property | Value |
---|---|
Density | 8 g/cm³ Show Supplier Material materials with Density of 8 g/cm³ |
Mechanical
Property | Value |
---|---|
Elastic modulus | 230 GPa Show Supplier Material materials with Elastic modulus of 230 GPa |
Hardness, Rockwell C | 58 - 65 [-] Show Supplier Material materials with Hardness, Rockwell C of 58 - 65 [-] |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100 °C | 1.15e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.15e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.17e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.17e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.22e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.22e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.24e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.24e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.27e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.27e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.3e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.3e-05 1/K | for 20°C to the mentioned temperature | |
700 °C | 1.29e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.29e-05 1/K | for 20°C to the mentioned temperature | |
Specific heat capacity | 420 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 420 J/(kg·K) | ||
Thermal conductivity | 20 °C | 24.3 W/(m·K) Show Supplier Material materials with Thermal conductivity of 24.3 W/(m·K) |
Electrical
Property | Value |
---|---|
Electrical resistivity | 5.4e-07 Ω·m Show Supplier Material materials with Electrical resistivity of 5.4e-07 Ω·m |
Chemical properties
Property | Value |
---|---|
Carbon | 1.3 % Show Supplier Material materials with Carbon of 1.3 % |
Chromium | 4.2 % Show Supplier Material materials with Chromium of 4.2 % |
Iron | Balance |
Molybdenum | 5 % Show Supplier Material materials with Molybdenum of 5 % |
Tungsten | 6.4 % Show Supplier Material materials with Tungsten of 6.4 % |
Vanadium | 3 % Show Supplier Material materials with Vanadium of 3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Thread-cutting tools, reamers, heavy-duty milling cutters, drills, punching tools |