General
Property | Value |
---|---|
Density | 7.9 g/cm³ Show Supplier Material materials with Density of 7.9 g/cm³ |
Mechanical
Property | Value |
---|---|
Elastic modulus | 250 GPa Show Supplier Material materials with Elastic modulus of 250 GPa |
Hardness, Rockwell C | 63 - 69 [-] Show Supplier Material materials with Hardness, Rockwell C of 63 - 69 [-] |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100 °C | 1.01e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.01e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.03e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.03e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.06e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.06e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.08e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.08e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.11e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.11e-05 1/K | for 20°C to the mentioned temperature | |
Specific heat capacity | 420 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 420 J/(kg·K) | ||
Thermal conductivity | 20 °C | 22.5 W/(m·K) Show Supplier Material materials with Thermal conductivity of 22.5 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbon | 2.3 % Show Supplier Material materials with Carbon of 2.3 % |
Chromium | 4.2 % Show Supplier Material materials with Chromium of 4.2 % |
Cobalt | 10.5 % Show Supplier Material materials with Cobalt of 10.5 % |
Iron | Balance |
Molybdenum | 7 % Show Supplier Material materials with Molybdenum of 7 % |
Tungsten | 7 % Show Supplier Material materials with Tungsten of 7 % |
Vanadium | 6.5 % Show Supplier Material materials with Vanadium of 6.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Heavy-duty cutting tools with very high requirements on red hardness and wear resistance |