General
Property | Value |
---|---|
Bulk density | 3.8 - 4.6 g/cm³ Show Supplier Material materials with Bulk density of 3.8 - 4.6 g/cm³ |
Particle size range | 20 - 53 µm Show Supplier Material materials with Particle size range of 20 - 53 µm |
Mechanical
Property | Value | Comment |
---|---|---|
Elongation | 5 % Show Supplier Material materials with Elongation of 5 % | A5 |
Hardness, Rockwell C | 52 [-] Show Supplier Material materials with Hardness, Rockwell C of 52 [-] | |
Tensile strength | 2050 - 2150 MPa Show Supplier Material materials with Tensile strength of 2050 - 2150 MPa | |
Yield strength | 1980 - 2080 MPa Show Supplier Material materials with Yield strength of 1980 - 2080 MPa | RP02 |
Rheological Properties
Property | Value |
---|---|
Hall flow | 12 - 20 s/50g Show Supplier Material materials with Hall flow of 12 - 20 s/50g |
Chemical properties
Property | Value |
---|---|
Carbon | 0.02 % Show Supplier Material materials with Carbon of 0.02 % |
Cobalt | 13.5 % Show Supplier Material materials with Cobalt of 13.5 % |
Iron | Balance |
Manganese | 0.5 % Show Supplier Material materials with Manganese of 0.5 % |
Molybdenum | 5 % Show Supplier Material materials with Molybdenum of 5 % |
Nickel | 18 % Show Supplier Material materials with Nickel of 18 % |
Silicon | 0.5 % Show Supplier Material materials with Silicon of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive manufacturing | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Der Printdur® Powderfort can be processed on LPBF systems. The process parameters are similar to those of 1.2709. Please contact us for further information. |