Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Find Materials
Categories
Printdur® 2343
1.2343 is a tool steel used for 3D printing (additive manufacturing) purposes.
This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).
All categories
Bainidur 1300 – Special Steel for Distortion-free, Cost-efficient Forgings
Completion Tools Made of Corroplast 4418 Mod
Ferro-Titanit Nikrodur: The Key for Successful Pelletizing
Metal Powder Production - The Key to Successful 3D Printing
Plastic Mold Steel for the Medical Market
Remelting Steel for the Highest Demands: Electro Slag Remelting and Vacuum Arc Remelting
Special Steels for High Pressure Die Casting
Steel Technology Meets Oil & Gas Exploration Technology
Steels Used in the Automotive Industry
Thermodur 2383 Supercool — Hot Work Tool Steel for Press Hardening
Tool Steels for the Plastic Mold Industry
Turn Back the Time: Steel for Watches
Chemical properties
Property | Value |
---|---|
Carbon | 0.37 % Show Supplier Material materials with Carbon of 0.37 % |
Chromium | 5.5 % Show Supplier Material materials with Chromium of 5.5 % |
Iron | Balance |
Manganese | 0.5 % Show Supplier Material materials with Manganese of 0.5 % |
Molybdenum | 1.3 % Show Supplier Material materials with Molybdenum of 1.3 % |
Silicon | 1 % Show Supplier Material materials with Silicon of 1 % |
Vanadium | 0.4 % Show Supplier Material materials with Vanadium of 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive manufacturing |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
COMPANY
CONTACT US
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.