General
Property | Value |
---|---|
Bulk density | 3.8 - 4.6 g/cm³ Show Supplier Material materials with Bulk density of 3.8 - 4.6 g/cm³ |
Particle size range | 20 - 53 µm Show Supplier Material materials with Particle size range of 20 - 53 µm |
Mechanical
Property | Value | Comment |
---|---|---|
Charpy impact energy, V-notch | 100 J Show Supplier Material materials with Charpy impact energy, V-notch of 100 J | |
Elongation | 35 % Show Supplier Material materials with Elongation of 35 % | A5 |
Tensile strength | 920 - 1030 MPa Show Supplier Material materials with Tensile strength of 920 - 1030 MPa | |
Yield strength | 660 - 760 MPa Show Supplier Material materials with Yield strength of 660 - 760 MPa | RP02 |
Magnetic
Property | Value | Comment |
---|---|---|
Relative magnetic permeability | 1 [-] Show Supplier Material materials with Relative magnetic permeability of 1 [-] | max. | None magnetic |
Rheological Properties
Property | Value |
---|---|
Hall flow | 12 - 20 s/50g Show Supplier Material materials with Hall flow of 12 - 20 s/50g |
Chemical properties
Property | Value |
---|---|
Carbon | 0.03 % Show Supplier Material materials with Carbon of 0.03 % |
Chromium | 22 % Show Supplier Material materials with Chromium of 22 % |
Cobalt | 0.5 % Show Supplier Material materials with Cobalt of 0.5 % |
Iron | 5 % Show Supplier Material materials with Iron of 5 % |
Manganese | 0.5 % Show Supplier Material materials with Manganese of 0.5 % |
Molybdenum | 9 % Show Supplier Material materials with Molybdenum of 9 % |
Nickel | Balance |
Niobium | 3.5 % Show Supplier Material materials with Niobium of 3.5 % |
Silicon | 0.5 % Show Supplier Material materials with Silicon of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive manufacturing | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Printdur® Ni625 can be processed on LPBF systems. The process parameters are similar to those of alloy 625. Please contact us for further information. |