Acidur 4401

Alternative and trade names
Acidur 4401 Niro-Cut, Type 316/316L, F316/F316L
.XLSX
.PDF
Save

Properties

Electrical

Electrical resistivity ρel

7.5E-7 Ω·m at 20 °C

General

Density ρ

8 g/cm³ at 20 °C

Mechanical

Charpy impact energy aK,charpy

60 J at 20 °C

min

Elastic modulus E

200 GPa at 20 °C

Show chart

Elongation A2 A2

40 % at 20 °C

min

Elongation A5 A5

35 % at 20 °C

min

Hardness, HBW HBW

215 [-] at 20 °C

max

Hardness, Rockwell C HRC

22 [-] at 20 °C

max

Reduction of area Z

50 % at 20 °C

min

Tensile strength Rm

240 MPa at 20 °C

min

Yield strength Rp0.2 Rp0.2

205 MPa at 20 °C

min

Thermal

Coefficient of thermal expansion α

1.6E-5 1/K at 100 °C

Show chart

Specific heat capacity cp

500 J/(kg·K) at 20 °C

Thermal conductivity λ

15 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

-

balance

Cr

16.5 - 18 %

Ni

10 - 13 %

Mo

2 - 2.5 %

Mn

2 %

max

More

Technological properties

Processing history

Quenched

This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.