General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.45 g/cm³ Show Supplier Material materials with Density of 1.45 g/cm³ | dry | ISO 1183 |
Limiting oxygen index | 20 % Show Supplier Material materials with Limiting oxygen index of 20 % | dry | ISO 4589-1/-2 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Water absorption | 0.3 % Show Supplier Material materials with Water absorption of 0.3 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | -40 °C | 8.1 GPa Show Supplier Material materials with Elastic modulus of 8.1 GPa | dry | ISO 527-1/-2 |
7.2 GPa Show Supplier Material materials with Elastic modulus of 7.2 GPa | dry | ISO 527-1/-2 | ||
100 °C | 3.3 GPa Show Supplier Material materials with Elastic modulus of 3.3 GPa | dry | ISO 527-1/-2 | |
120 °C | 3 GPa Show Supplier Material materials with Elastic modulus of 3 GPa | dry | ISO 527-1/-2 | |
160 °C | 2.5 GPa Show Supplier Material materials with Elastic modulus of 2.5 GPa | dry | ISO 527-1/-2 | |
180 °C | 2.2 GPa Show Supplier Material materials with Elastic modulus of 2.2 GPa | dry | ISO 527-1/-2 | |
Elongation | -40 °C | 2.4 % Show Supplier Material materials with Elongation of 2.4 % | dry | ISO 527-1/-2 |
3 % Show Supplier Material materials with Elongation of 3 % | dry | ISO 527-1/-2 | ||
120 °C | 6.5 % Show Supplier Material materials with Elongation of 6.5 % | dry | ISO 527-1/-2 | |
160 °C | 6.7 % Show Supplier Material materials with Elongation of 6.7 % | dry | ISO 527-1/-2 | |
180 °C | 6.7 % Show Supplier Material materials with Elongation of 6.7 % | dry | ISO 527-1/-2 | |
Flexural modulus | 6.9 GPa Show Supplier Material materials with Flexural modulus of 6.9 GPa | dry | ISO 178 | |
120 °C | 3 GPa Show Supplier Material materials with Flexural modulus of 3 GPa | dry | ISO 178 | |
160 °C | 2.5 GPa Show Supplier Material materials with Flexural modulus of 2.5 GPa | dry | ISO 178 | |
Flexural yield strength | 190 MPa Show Supplier Material materials with Flexural yield strength of 190 MPa | dry | ISO 178 | |
120 °C | 85 MPa Show Supplier Material materials with Flexural yield strength of 85 MPa | dry | ISO 178 | |
160 °C | 65 MPa Show Supplier Material materials with Flexural yield strength of 65 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m² | dry | ISO 179/1eA |
23 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 35 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 35 kJ/m² | dry | ISO 179/1eU |
23 °C | 35 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 35 kJ/m² | dry | ISO 179/1eU | |
Tensile strength | -40 °C | 155 MPa Show Supplier Material materials with Tensile strength of 155 MPa | dry | ISO 527-1/-2 |
120 MPa Show Supplier Material materials with Tensile strength of 120 MPa | dry | ISO 527-1/-2 | ||
100 °C | 65 MPa Show Supplier Material materials with Tensile strength of 65 MPa | dry | ISO 527-1/-2 | |
120 °C | 60 MPa Show Supplier Material materials with Tensile strength of 60 MPa | dry | ISO 527-1/-2 | |
160 °C | 45 MPa Show Supplier Material materials with Tensile strength of 45 MPa | dry | ISO 527-1/-2 | |
180 °C | 38 MPa Show Supplier Material materials with Tensile strength of 38 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 4e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
8e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Heat deflection temperature | 205 °C Show Supplier Material materials with Heat deflection temperature of 205 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 225 °C Show Supplier Material materials with Melting point of 225 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | dry | UL746B | 0.75 mm | ||
Thermal diffusivity | 1.11e-07 mm²/s Show Supplier Material materials with Thermal diffusivity of 1.11e-07 mm²/s | dry | - |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 400 V Show Supplier Material materials with Comparative tracking index of 400 V | dry | IEC 60112 | |
Dielectric constant | 3.5 [-] Show Supplier Material materials with Dielectric constant of 3.5 [-] | dry | IEC 62631-2-1 | 1MHz |
3.7 [-] Show Supplier Material materials with Dielectric constant of 3.7 [-] | dry | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 30 kV/mm Show Supplier Material materials with Dielectric strength of 30 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 20 [-] Show Supplier Material materials with Dissipation factor of 20 [-] | dry | IEC 62631-2-1 | 100Hz |
180 [-] Show Supplier Material materials with Dissipation factor of 180 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 1220 g/cm³ Show Supplier Material materials with Density of melt of 1220 g/cm³ | dry | - | ||
Melt volume-flow rate | 250 °C | 23 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 23 cm³/10min | dry | ISO 1133 | |
Shrinkage | 0.45 % Show Supplier Material materials with Shrinkage of 0.45 % | dry | Sim. to ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Shrinkage of 1.3 % | dry | Sim. to ISO 294-4 | Normal | ||
Specific heat capacity melt | 1850 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1850 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.25 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.25 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 20% Glass Fiber |