Hiperco 50A Bar

.XLSX
.PDF
Save

Description

An alloy of 49% cobalt, and 2% vanadium, balance iron, Hiperco 50 and Hiperco 50A have the highest magnetic saturation of all soft-magnetic alloys and excel in applications where this attribute is needed. Hiperco 50 maintains its strength after heat treating making it your best choice for applications that experience high forces (e.g. rotating parts).

Related Standards

Equivalent Materials

Properties

General

Density ρ

8.12 g/cm³ at 20 °C

Dimension

Dimensions

Available widths: 13.0mm, 19.3mm, 25.4mm, 25.7mm, 32.0mm, 38.4mm, 51.2mm, 63.5mm, 69.9mm, 76.2mm

Length l

3050 - 3660 mm

Mill random length

Width w

13 - 76.2 mm

Mechanical

Elastic modulus E

207 GPa at 20 °C

Elongation A

7 % at 20 °C

in 2 in.

Hardness, Rockwell B HRB

20 [-] at 20 °C

Tensile strength Rm

717 MPa at 20 °C

Yield strength YS

365 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

9.5E-5 1/K at 200 °C

Show chart

Melting point Tm

1427 °C

Specific heat capacity cp

420 J/(kg·K) at 20 °C

Thermal conductivity λ

29 W/(m·K) at 20 °C

Electrical

Electrical resistivity ρel

4E-7 Ω·m at 20 °C

Magnetic

Curie temperature Tc

940 °C

Chemical properties

Element

Weight %

Comment

Fe

49.15 %

Co

48.75 %

V

2 %

Ni

0.25 %

Cr

0.15 %

More

Technological properties

Application areas

Special Motors for the Aerospace Industry (e.g. applications where high magnetic saturation and high strength is required with as little weight as possible); Electromagnets for medical applications (e.g. to focus beams for radiation therapy in medical radiology applications); Electrical Generators; Specialty Transformers (e.g. electrical circuits and magnetic circuits where frequencies must be varied); Pole Pieces for Electromagnets; Magnetic Bearings (e.g. applications where rotating parts are levitated); High Magnetic Flux Devices and Instruments.

This material data has been provided by Ed Fagan.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.