General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.36 g/cm³ Show Material materials with Density of 8.36 g/cm³ |
Dimension
Property | Value |
---|---|
Length | 1828 mm Show Material materials with Length of 1828 mm |
Thickness | 0.25 - 3.2 mm Show Material materials with Thickness of 0.25 - 3.2 mm |
Width | 330.2 mm Show Material materials with Width of 330.2 mm |
Dimensions | Available thicknesses: 0.3mm, 0.4mm, 0.5mm, 0.6mm, 0.8mm, 0.9mm, 1.0mm, 1.3mm, 1.5mm, 2.1mm, 2.3mm, 2.5mm, 3.2mm |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 207 GPa Show Material materials with Elastic modulus of 207 GPa | |
Elongation | 23.0 °C | 30 % Show Material materials with Elongation of 30 % | in 2 in. |
Hardness, Rockwell B | 23.0 °C | 80 [-] Show Material materials with Hardness, Rockwell B of 80 [-] | |
Tensile strength | 23.0 °C | 518 MPa Show Material materials with Tensile strength of 518 MPa | |
Yield strength | 23.0 °C | 276 MPa Show Material materials with Yield strength of 276 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 5.8E-6 1/K Show Material materials with Coefficient of thermal expansion of 5.8E-6 1/K | from 30°C to the mentioned temperature |
150.0 °C | 5.6E-6 1/K Show Material materials with Coefficient of thermal expansion of 5.6E-6 1/K | from 30°C to the mentioned temperature | |
200.0 °C | 5.4E-6 1/K Show Material materials with Coefficient of thermal expansion of 5.4E-6 1/K | from 30°C to the mentioned temperature | |
250.0 °C | 5.3E-6 1/K Show Material materials with Coefficient of thermal expansion of 5.3E-6 1/K | from 30°C to the mentioned temperature | |
300.0 °C | 5.1E-6 1/K Show Material materials with Coefficient of thermal expansion of 5.1E-6 1/K | from 30°C to the mentioned temperature | |
350.0 °C | 4.9E-6 1/K Show Material materials with Coefficient of thermal expansion of 4.9E-6 1/K | from 30°C to the mentioned temperature | |
400.0 °C | 4.6E-6 - 5.2E-6 1/K Show Material materials with Coefficient of thermal expansion of 4.6E-6 - 5.2E-6 1/K | from 30°C to the mentioned temperature | |
450.0 °C | 5.1E-6 - 5.5E-6 1/K Show Material materials with Coefficient of thermal expansion of 5.1E-6 - 5.5E-6 1/K | from 30°C to the mentioned temperature | |
500.0 °C | 6.1E-6 1/K Show Material materials with Coefficient of thermal expansion of 6.1E-6 1/K | from 30°C to the mentioned temperature | |
550.0 °C | 6.8E-6 1/K Show Material materials with Coefficient of thermal expansion of 6.8E-6 1/K | from 30°C to the mentioned temperature | |
600.0 °C | 7.5E-6 1/K Show Material materials with Coefficient of thermal expansion of 7.5E-6 1/K | from 30°C to the mentioned temperature | |
700.0 °C | 8.7E-6 1/K Show Material materials with Coefficient of thermal expansion of 8.7E-6 1/K | from 30°C to the mentioned temperature | |
800.0 °C | 1.03E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.03E-5 1/K | from 30°C to the mentioned temperature | |
900.0 °C | 1.08E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.08E-5 1/K | from 30°C to the mentioned temperature | |
1026.0 °C | 1.17E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.17E-5 1/K | from 30°C to the mentioned temperature | |
Melting point | 1449 °C Show Material materials with Melting point of 1449 °C | ||
Specific heat capacity | 23.0 °C | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) | |
Thermal conductivity | 23.0 °C | 17 W/(m·K) Show Material materials with Thermal conductivity of 17 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 23.0 °C | 4E-7 Ω·m Show Material materials with Electrical resistivity of 4E-7 Ω·m |
Magnetic
Property | Value |
---|---|
Curie temperature | 435 °C Show Material materials with Curie temperature of 435 °C |
Chemical properties
Property | Value |
---|---|
Carbon | 0.02 % Show Material materials with Carbon of 0.02 % |
Chromium | 0.2 % Show Material materials with Chromium of 0.2 % |
Cobalt | 17 % Show Material materials with Cobalt of 17 % |
Iron | Balance |
Nickel | 29 % Show Material materials with Nickel of 29 % |
Silicon | 0.2 % Show Material materials with Silicon of 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Common applications of Kovar: Glass-to-metal hermetic sealing with hard borosilicate glass, ceramic-to-metal sealing, power tubes, microwave tubes, transistors, diodes, integrated circuits, hybrid packages |