Nickel 205 Sheet

.XLSX
.PDF
Save

Description

Commercially pure, unalloyed Nickel.

Related Standards

Equivalent Materials

Properties

General

Density ρ

8.89 g/cm³ at 20 °C

Dimension

Dimensions

Available thicknesses: 0.76mm, 1.27mm, 1.57mm, 3.18mm

Thickness t

0.76 - 3.18 mm

Mechanical

Elastic modulus E

207 GPa at 20 °C

Elongation A

40 % at 20 °C

in 2 in.

Hardness, Rockwell B HRB

80 [-] at 20 °C

Tensile strength Rm

449 MPa at 20 °C

Yield strength YS

138 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.3E-5 1/K at 100 °C

Melting point Tm

1440 °C

Specific heat capacity cp

452 J/(kg·K) at 20 °C

Thermal conductivity λ

75 W/(m·K) at 20 °C

Electrical

Electrical resistivity ρel

9.5E-8 Ω·m at 20 °C

Magnetic

Curie temperature Tc

360 °C

Chemical properties

Element

Weight %

Comment

Ni

99.5 %

Fe

0.2 %

Si

0.15 %

C

0.07 %

Ti

0.05 %

More

Technological properties

Application areas

Common applications of Nickel 205: Getter tabs, heating element sheathing, anodes, fuel cells, special purpose electron tubes, transistor enclosures, cathode shields, spark gaps

This material data has been provided by Ed Fagan.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.