Many practical applications of tungsten are based on its high melting point and density and its low vapor pressure. Tungsten is an excellent material for high vacuum technology, dimensional stability, glass seals and furnace construction. In addition, tungsten’s high density gives it a capacity to absorb radioactive radiation. Tungsten has found wide use as additives to steel to enhance physical properties and an alloy with nickel, copper and iron to provide high density machinable materials.

Equivalent Materials

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

19.3 g/cm³

Show Material materials with Density of 19.3 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

400 GPa

Show Material materials with Elastic modulus of 400 GPa

Hardness, Vickers

23.0 °C

460 [-]

Show Material materials with Hardness, Vickers of 460 [-]

Tensile strength

20.0 °C

1725 MPa

Show Material materials with Tensile strength of 1725 MPa

500.0 °C

1035 MPa

Show Material materials with Tensile strength of 1035 MPa

1000.0 °C

515 MPa

Show Material materials with Tensile strength of 515 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

4.2E-6 1/K

Show Material materials with Coefficient of thermal expansion of 4.2E-6 1/K

Melting point

3420 °C

Show Material materials with Melting point of 3420 °C

Specific heat capacity

23.0 °C

134 J/(kg·K)

Show Material materials with Specific heat capacity of 134 J/(kg·K)

Thermal conductivity

23.0 °C

173 W/(m·K)

Show Material materials with Thermal conductivity of 173 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

5.28E-8 Ω·m

Show Material materials with Electrical resistivity of 5.28E-8 Ω·m

Chemical properties

PropertyValueComment

Tungsten

99.95 %

Show Material materials with Tungsten of 99.95 %

min

Technological properties

Property
Application areas

Common applications of Tungsten: Lamp filaments, high temperature furnaces, welding electrodes