Description

PP (Polypropylene) filled with detectable filler. Main features : detectable via metal detector , x-ray detectable, Explanation of food contact according to FDA and EU 10/2011 on request

This material data has been provided by Ensinger GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

0.68 g/cm³

Show Supplier Material materials with Bulk density of 0.68 g/cm³

EN ISO 60

Density

23.0 °C

1.28 g/cm³

Show Supplier Material materials with Density of 1.28 g/cm³

Water absorption

23.0 °C

0.1 %

Show Supplier Material materials with Water absorption of 0.1 %

DIN EN ISO 62, 23 °C / 50 % relative humidity up to saturation

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.2 GPa

Show Supplier Material materials with Elastic modulus of 2.2 GPa

DIN EN ISO 527-1, 50mm/min

Elongation

23.0 °C

30 %

Show Supplier Material materials with Elongation of 30 %

DIN EN ISO 527-1, 50mm/min

Flexural modulus

23.0 °C

1.8 GPa

Show Supplier Material materials with Flexural modulus of 1.8 GPa

DIN EN ISO 178

Impact strength, Charpy unnotched

23.0 °C

20 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 20 kJ/m²

DIN EN ISO 179-1eU

Tensile strength

23.0 °C

25 MPa

Show Supplier Material materials with Tensile strength of 25 MPa

DIN EN ISO 527-1, 50mm/min

Flexural strain

DIN EN ISO 178

Flexural strength

DIN EN ISO 178

Thermal

PropertyValueComment

Glass transition temperature

13 °C

Show Supplier Material materials with Glass transition temperature of 13 °C

Max service temperature, long

100 °C

Show Supplier Material materials with Max service temperature, long of 100 °C

Max service temperature, short

130 °C

Show Supplier Material materials with Max service temperature, short of 130 °C

Melting point

165 °C

Show Supplier Material materials with Melting point of 165 °C

DIN 53765

Flammability

UL94 class HB, DIN IEC 60695-11-10

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

39 g/10min

Show Supplier Material materials with Melt mass-flow rate of 39 g/10min

DIN EN ISO 1133, 230°C/2.16kg

Melt volume-flow rate

37 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 37 cm³/10min

DIN EN ISO 1133, 230°C/2.16kg

Shrinkage

23.0 °C

1.4 %

Show Supplier Material materials with Shrinkage of 1.4 %

DIN EN ISO 294-4

Shrinkage, transverse

23.0 °C

1.54 %

Show Supplier Material materials with Shrinkage, transverse of 1.54 %

DIN EN ISO 294-4

Technological properties

Property
Certifications

Explanation of food contact according to FDA and EU 10/2011

Color

Blue

Detectability

Inductive: 6 mm Al, X-Ray detectable: 3.5 mm Al

Fillers

Detectable Filler

Processing methods

Permissible residual moisture content (%): 0.1, drying temperature (°C): 100, drying time (h): 2, mould temperature (°C): 100, material temperature (°C): 250, cylinder/processing temperature (°C): 260