EPLAMID 6 IMP NC Q1A801 (PA6)

Want to keep this datasheet? Save it now in your required format

Description

Unreinforced and modified polyamide 6 improved with good-impact resistance, heat stabilized and lubricated for injection molding.

Eplamid 6 Impact modified compounds are used in all sectors of industry, offering a good impact strength for mechanical properties and ensures an outstanding performance even at low temperatures (up to -40°C).

This material data has been provided by Epsan.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.09 g/cm³

Show Supplier Material materials with Density of 1.09 g/cm³

ISO 1183

Water content

23.0 °C

0.1 %

Show Supplier Material materials with Water content of 0.1 %

ISO 15512

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.2 GPa

Show Supplier Material materials with Elastic modulus of 2.2 GPa

ISO 527-2 (1mm/min)

Elongation

23.0 °C

45 %

Show Supplier Material materials with Elongation of 45 %

min., ISO 527-2 (5mm/min)

Flexural modulus

23.0 °C

1.95 GPa

Show Supplier Material materials with Flexural modulus of 1.95 GPa

ISO 178 (2mm/min)

Flexural strength

23.0 °C

80 MPa

Show Supplier Material materials with Flexural strength of 80 MPa

ISO 178 (2mm/min)

Impact strength, Charpy notched

-30.0 °C

18 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 18 kJ/m²

ISO 179/1eA

23.0 °C

20 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-40.0 °C

14 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 14 kJ/m²

ISO 180/1A

23.0 °C

18 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 18 kJ/m²

ISO 180/1A

Unlock all property charts

Tensile strength

23.0 °C

55 MPa

Show Supplier Material materials with Tensile strength of 55 MPa

ISO 527-2 (5mm/min)

Impact strength, Charpy unnotched

no break at 23°C; ISO 179/1eU

Impact strength, Izod unnotched

no break at 23°C; ISO 180/1U

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

150 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 150 °C

ISO 75-2/B

Heat deflection temperature, 1.80 MPa

55 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 55 °C

ISO 75-2/A

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

ISO 3146

Flammability

UL94 (0.8mm) HB, EN 60695-11-10

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

EN 60112

Surface resistivity

23.0 °C

1.00E+13 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

1.4 %

Show Supplier Material materials with Shrinkage of 1.4 %

ISO 294-4 (3mm)

Shrinkage, transverse

23.0 °C

2 %

Show Supplier Material materials with Shrinkage, transverse of 2 %

ISO 294-4 (3mm)

Technological properties

Property
Application areas

Eplamid 6 Impact modified compounds are used in all sectors of industry, offering a good impact strength for mechanical properties and ensures an outstanding performance even at low temperatures (up to -40°C).

Other

Laboratory conditions are 23 ±2°C and 45-55 % RH.