General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.08 g/cm³ Show Supplier Material materials with Density of 1.08 g/cm³ | ISO 1183 |
Water content | 23.0 °C | 0.1 % Show Supplier Material materials with Water content of 0.1 % | ISO 15512 |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastic modulus of 2.2 GPa | ISO 527-2 (1mm/min) | ||
Elongation | 23.0 °C | 50 % Show Supplier Material materials with Elongation of 50 % | min., ISO 527-2 (5mm/min) | ||
Flexural modulus | 23.0 °C | 1.9 GPa Show Supplier Material materials with Flexural modulus of 1.9 GPa | ISO 178 (2mm/min) | ||
Flexural strength | 23.0 °C | 70 MPa Show Supplier Material materials with Flexural strength of 70 MPa | ISO 178 (2mm/min) | ||
Impact strength, Charpy notched | -30.0 °C | 22 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 22 kJ/m² | ISO 179/1eA | ||
23.0 °C | 70 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 70 kJ/m² | ISO 179/1eA | |||
Impact strength, Izod notched | -40.0 °C | 18 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 18 kJ/m² | ISO 180/1A | ||
23.0 °C | 65 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 65 kJ/m² | ISO 180/1A | |||
Tensile strength | 23.0 °C | 45 MPa Show Supplier Material materials with Tensile strength of 45 MPa | ISO 527-2 (5mm/min) | ||
Impact strength, Charpy unnotched | no break at 23°C; ISO 179/1eU | ||||
Impact strength, Izod unnotched | no break at 23°C; ISO 180/1U |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 145 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 145 °C | ISO 75-2/B | |
Heat deflection temperature, 1.80 MPa | 50 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 50 °C | ISO 75-2/A | |
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | ISO 3146 | |
Flammability | UL94 (0.8mm) HB, EN 60695-11-10 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | EN 60112 |
Surface resistivity | 23.0 °C | 1.00E+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq | ASTM D257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Eplamid 6 Impact modified compounds are used in all sectors of industry, offering a good impact strength for mechanical properties and ensures an outstanding performance even at low temperatures (up to -40°C). | |
Other | Laboratory conditions are 23 ±2°C and 45-55 % RH. |