General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 3.7 g/cm³ Show Supplier Material materials with Density of 3.7 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 400 GPa Show Supplier Material materials with Elastic modulus of 400 GPa |
Flexural strength | 23.0 °C | 650 MPa Show Supplier Material materials with Flexural strength of 650 MPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 8 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 8 MPa·√m |
Poisson's ratio | 23.0 °C | 0.2 [-] Show Supplier Material materials with Poisson's ratio of 0.2 [-] |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1000.0 °C | 6.8E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 6.8E-6 1/K | |
Max service temperature | 1500 °C Show Supplier Material materials with Max service temperature of 1500 °C | in inert gas | |
Max service temperature, long | 1550 °C Show Supplier Material materials with Max service temperature, long of 1550 °C | in air | |
Thermal conductivity | 23.0 °C | 35 W/(m·K) Show Supplier Material materials with Thermal conductivity of 35 W/(m·K) | |
Thermal shock parameter R1 | 191 °C Show Supplier Material materials with Thermal shock parameter R1 of 191 °C | ||
Thermal shock parameter R2 | 6691 W/m Show Supplier Material materials with Thermal shock parameter R2 of 6691 W/m |