Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

15.2 g/cm³

Show Supplier Material materials with Density of 15.2 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

520 GPa

Show Supplier Material materials with Elastic modulus of 520 GPa

Flexural strength

23.0 °C

710 MPa

Show Supplier Material materials with Flexural strength of 710 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

1000.0 °C

6.1E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 6.1E-6 1/K

Max service temperature

2300 °C

Show Supplier Material materials with Max service temperature of 2300 °C

in inert gas

Max service temperature, long

500 °C

Show Supplier Material materials with Max service temperature, long of 500 °C

in air