The Extrudr TPU Flex line, which features Extrudr TPU Flex in varying degrees of hardness, has been developed mainly for use with industrial machinery.

Properties

General

Density ρ

1.15 g/cm³ at 20 °C

ISO 2781

Mechanical

Breaking stress Sbreak

475 % at 20 °C

ISO 527-2

Hardness, Shore A HS A

98 [-] at 20 °C

ISO 868

Tear Strength Unnicked Rtear,unnicked

176 kN/m at 20 °C

ISO 34-1B

Tensile strength Rm

42 MPa at 20 °C

ISO 527-2

Thermal

Melting point Tm

180 - 200 °C

ISO 3146-C

Vicat softening temperature Tsoft

110 °C

ISO 306

Technological properties

Application areas

Due to its chemical and mechanical resistance, TPU is primarily used in the car and footwear industry.

Handling recommendations

Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year.

This material data has been provided by extrudr.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.