Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 - 1.3 % Show Supplier Material materials with Aluminium of 0.3 - 1.3 % |
Copper | 59 - 61.5 % Show Supplier Material materials with Copper of 59 - 61.5 % |
Iron | 1 % Show Supplier Material materials with Iron of 1 % |
Lead | 1 % Show Supplier Material materials with Lead of 1 % |
Manganese | 0.6 - 1.8 % Show Supplier Material materials with Manganese of 0.6 - 1.8 % |
Nickel | 0.6 % Show Supplier Material materials with Nickel of 0.6 % |
Silicon | 0.5 % Show Supplier Material materials with Silicon of 0.5 % |
Tin | 0.3 % Show Supplier Material materials with Tin of 0.3 % |
Zinc | Balance, REM |