Chemical properties
Property | Value |
---|---|
Aluminium | 5 - 6 % Show Supplier Material materials with Aluminium of 5 - 6 % |
Copper | 63 - 65 % Show Supplier Material materials with Copper of 63 - 65 % |
Iron | 2 - 3.5 % Show Supplier Material materials with Iron of 2 - 3.5 % |
Lead | 0.2 - 0.8 % Show Supplier Material materials with Lead of 0.2 - 0.8 % |
Manganese | 3.5 - 5 % Show Supplier Material materials with Manganese of 3.5 - 5 % |
Nickel | 0.5 % Show Supplier Material materials with Nickel of 0.5 % |
Silicon | 0.2 % Show Supplier Material materials with Silicon of 0.2 % |
Tin | 0.2 % Show Supplier Material materials with Tin of 0.2 % |
Zinc | Balance, REM |