Chemical properties
Property | Value |
---|---|
Aluminium | 0.1 % Show Supplier Material materials with Aluminium of 0.1 % |
Copper | 56.5 - 58.5 % Show Supplier Material materials with Copper of 56.5 - 58.5 % |
Iron | 0.2 - 1.2 % Show Supplier Material materials with Iron of 0.2 - 1.2 % |
Lead | 0.8 - 1.6 % Show Supplier Material materials with Lead of 0.8 - 1.6 % |
Manganese | 0.8 - 1.8 % Show Supplier Material materials with Manganese of 0.8 - 1.8 % |
Nickel | 0.3 % Show Supplier Material materials with Nickel of 0.3 % |
Tin | 0.2 - 1 % Show Supplier Material materials with Tin of 0.2 - 1 % |
Zinc | Balance, REM |