Description

DENSITEC-L is used for production of liquid phase sintered SiC and is a spray granulated powder based on our standard black SINTEX 13C. The powder is doped with oxides, temporary binders and pressing aids, and is ready to be pressed into a green body.

This material data has been provided by Fiven GmbH.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Bulk density

23.0 °C

0.86 g/cm³

Show Supplier Material materials with Bulk density of 0.86 g/cm³

Density

23.0 °C

3.21 g/cm³

Show Supplier Material materials with Density of 3.21 g/cm³

Particle size range

100 µm

Show Supplier Material materials with Particle size range of 100 µm

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

24 GPa

Show Supplier Material materials with Elastic modulus of 24 GPa

Plane-Strain Fracture Toughnes

23.0 °C

4.5 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4.5 MPa·√m

Rheological Properties

PropertyTemperatureValue

Hall flow

23.0 °C

22.5 s/50g

Show Supplier Material materials with Hall flow of 22.5 s/50g

Technological properties

Property
Application areas

Silicon Carbide Ready-To-Press granules for solid-state (SSiC) sintered technical ceramics.

Chemical composition

SiC type: SINTEX 13C; Al2O3: 5,5%; Y2O3: 3,5%; Moisture content: 1%; Binder content (total organic): 6%