Description

In certain applications, the use of higher-strength cast plates is not sufficient; high-strength rolled plates must be used. However, the problem with rolled plates is the wide toleration of thickness and flatness, which results in extremely complex processing. Precision rolled plate G.AL® 7075GF from alloy EN AW 7075 (AlZn5.5MgCu), finely milled on both sides and covered with protective foil, provides users with a semi-finished product which drastically reduces the time required for machining.

Primary standard name

Properties

Electrical

Electrical conductivity σel

1.90E+7 - 2.30E+7 S/m at 20 °C

General

Density ρ

2.8 g/cm³ at 20 °C

Surface roughness RMS

400 µm

Mechanical

Elastic modulus E

71 GPa at 20 °C

Elongation A50 A50

5 - 8 % at 20 °C

Hardness, HBW HBW

158 - 161 [-] at 20 °C

Test method: 2.5/62.5

Tensile strength Rm

530 - 540 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

460 - 470 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

2.34E-5 1/K at 20 °C

Specific heat capacity cp

862 J/(kg·K) at 20 °C

Thermal conductivity λ

130 - 160 W/(m·K) at 20 °C

Technological properties

Dimension

Standard stock sizes: 1520mm x 3020mm and 12-40mm in thickness

Other

Heat treatable alloy

Processing history

Temper: T651

This material data has been provided by Gleich Aluminum.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.