General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.8 g/cm³ Show Supplier Material materials with Density of 2.8 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 70 GPa Show Supplier Material materials with Elastic modulus of 70 GPa | |
Elongation | 23.0 °C | 5 - 8 % Show Supplier Material materials with Elongation of 5 - 8 % | |
Hardness, HBW | 23.0 °C | 110 - 115 [-] Show Supplier Material materials with Hardness, HBW of 110 - 115 [-] | Test method: 2.5/62.5 |
Tensile strength | 23.0 °C | 350 - 370 MPa Show Supplier Material materials with Tensile strength of 350 - 370 MPa | |
Yield strength Rp0.2 | 23.0 °C | 290 - 330 MPa Show Supplier Material materials with Yield strength Rp0.2 of 290 - 330 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.33E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.33E-5 1/K |
Specific heat capacity | 23.0 °C | 875 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 875 J/(kg·K) |
Thermal conductivity | 23.0 °C | 125 - 155 W/(m·K) Show Supplier Material materials with Thermal conductivity of 125 - 155 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 2.10E+7 - 2.40E+7 S/m Show Supplier Material materials with Electrical conductivity of 2.10E+7 - 2.40E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Non heat treatable | |
Processing history | Temper: T79 |