Description

Alumina content over 98% was developed for abrasive resistance and mechanical strength in chemically aggressive environments. This material features as below


  • Excellent resistance to corrosion and chemical attack
  • High wearing and abrasion resistant
  • Dense, non-porous and vacuum tight
  • This material data has been provided by Innovacera.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    3.9 g/cm³

    Show Supplier Material materials with Density of 3.9 g/cm³

    Mechanical

    PropertyTemperatureValue

    Compressive strength

    23.0 °C

    2500 MPa

    Show Supplier Material materials with Compressive strength of 2500 MPa

    Elastic modulus

    23.0 °C

    360 GPa

    Show Supplier Material materials with Elastic modulus of 360 GPa

    Flexural strength

    23.0 °C

    350 MPa

    Show Supplier Material materials with Flexural strength of 350 MPa

    Hardness, Vickers

    23.0 °C

    1764 [-]

    Show Supplier Material materials with Hardness, Vickers of 1764 [-]

    Plane-Strain Fracture Toughnes

    23.0 °C

    4 - 5 MPa·√m

    Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4 - 5 MPa·√m

    Poisson's ratio

    23.0 °C

    0.23 [-]

    Show Supplier Material materials with Poisson's ratio of 0.23 [-]

    Thermal

    PropertyTemperatureValue

    Coefficient of thermal expansion

    23.0 °C

    8.2E-6 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 8.2E-6 1/K

    Specific heat capacity

    23.0 °C

    800 J/(kg·K)

    Show Supplier Material materials with Specific heat capacity of 800 J/(kg·K)

    Thermal conductivity

    23.0 °C

    30 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 30 W/(m·K)

    Thermal shock parameter R2

    220 W/m

    Show Supplier Material materials with Thermal shock parameter R2 of 220 W/m

    Electrical

    PropertyTemperatureValue

    Dielectric constant

    23.0 °C

    9.8 [-]

    Show Supplier Material materials with Dielectric constant of 9.8 [-]

    Dielectric strength

    23.0 °C

    17 kV/mm

    Show Supplier Material materials with Dielectric strength of 17 kV/mm

    Electrical resistivity

    23.0 °C

    1.00E+20 Ω·m

    Show Supplier Material materials with Electrical resistivity of 1.00E+20 Ω·m

    Loss tangent

    23.0 °C

    1E-4 [-]

    Show Supplier Material materials with Loss tangent of 1E-4 [-]

    Technological properties

    Property
    Application areas

    Wear ceramic parts: Ceramic Nozzles, Ceramic, Sprayers Cyclones, Homogenising devices, Ceramic Linings, Milling Systems, Ceramic Thread guides - Precision components: Ceramic Measuring Components, Ceramic Control systems, (Micro) dosing valves, Electronic Components, Mechatronics, Optical applications - Machine-construction: Positioning Guide parts, Coatings, Transport ceramic rollers, Ceramic Dies, Textile machine parts, Furnace parts - Rotating equipment: Ceramic Sliding Bearings, Ceramic Ball bearings, Mechanical seals, Ceramic Plungers, Ceramic Valves / fittings, Dosing components - Cutting & moulding: Ceramic knives, Metal-forming tools, Seaming rolls, Ceramic Punches, Drawing dies

    Processing methods

    Cold Isostatic Press, Dry Press, Tape Casting, Precision Machining Processing