Dimension
Property | Value |
---|---|
Thickness | 0.03 mm Show Material materials with Thickness of 0.03 mm |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 5 GPa Show Material materials with Elastic modulus of 5 GPa | ISO 527 |
Elastic modulus, transverse | 23.0 °C | 4.5 GPa Show Material materials with Elastic modulus, transverse of 4.5 GPa | ISO 527 |
Elongation | 23.0 °C | 100 % Show Material materials with Elongation of 100 % | ISO 527 |
Elongation, transverse | 23.0 °C | 10 % Show Material materials with Elongation, transverse of 10 % | ISO 527 |
Tensile strength | 23.0 °C | 100 MPa Show Material materials with Tensile strength of 100 MPa | ISO 527 |
Tensile strength, transverse | 23.0 °C | 80 MPa Show Material materials with Tensile strength, transverse of 80 MPa | ISO 527 |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical insulation, printed circuit substrates, high temperature labels, flexible surface heaters, proven temperature resistance to use of lead free solders, acoustic speaker diaphragms, pressure sensor membranes | |
Certifications | APTIV® film is FDA and EU approved for food contact and is RoHS compliant. | |
Other | The key features are: High heat resistance, broad chemical resistance, excellent barrier properties, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent acoustic properties, high purity, lightweight, recyclable, easy to process. The APTIV 1100 series offers an improved thermal conductivity over APTIV 1000 films. | |
Processing methods | Can be laminated to other materials, thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated. |