Polyvinylidenefluoride (PVDF) Granules are fluorinated thermoplastic homopolymers for injection molding, with outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo-mechanical properties.

Properties

General

Density ρ

1.78 g/cm³ at 20 °C

ISO 1183

Limiting oxygen index LOI

43 % at 20 °C

ISO 4589-2

Melt mass-flow rate MFR

17.8 g/10min at 360 °C

ISO 1183 (10kg)

Shrinkage cshrink

2 % at 20 °C

ISO 294-4 (molding)

Shrinkage, transverse cshrink, trans

2 % at 20 °C

ISO 294-4 (molding)

Water absorption, equilibrium cwater,equib

0.02 % at 20 °C

ISO 62, 50%RH

Water absorption, saturation cwater,sat

0.03 % at 23 °C

ISO 62

Mechanical

Elastic modulus E

2.2 GPa at 23 °C

ISO 527-2

Elongation A

50 % at 20 °C

ISO 527-2

Impact strength, Charpy notched Ivnot

8 kJ/m² at 20 °C

ISO 179/1eA

Impact strength, Charpy unnotched Iunnot

210 kJ/m² at 20 °C

ISO 179/1eA

Yield strength YS

54 MPa at 23 °C

ISO 527-2

Thermal

Coefficient of thermal expansion α

1.5000000000000001E-4 1/K at 20 °C

ISO 11359-2

Flammability

IEC 60695-11-10, -20 V-0 (0.8mm, 1.6mm)

Glass transition temperature Tg

-40 °C

ISO 11357-2 (10°C/min)

Heat deflection temperature, 1.80 MPa HDT1.8,MPa

110 °C

ISO 75-2/A

Vicat softening temperature Tsoft

139 °C

ISO 306/B50

Electrical

Comparative tracking index CTI

600 V at 20 °C

IEC 60112

Dielectric constant, 100Hz εr,100Hz

9 [-] at 20 °C

IEC 60250

Dielectric constant, 1MHz εr,1MHz

7 [-] at 20 °C

IEC 60250

Dielectric strength EDS

21 kV/mm at 20 °C

IEC 60243-1

Dissipation factor, 1MHz ε''1MHz

0.21 [-] at 20 °C

IEC 60250

Electrical resistivity ρel

2.00E+12 Ω·m at 20 °C

IEC 60093

Sheet resistivity ρel,sheet

1.00E+15 Ω/sq at 20 °C

IEC 60093

Technological properties

Application areas

Corrosion protection in the chemical industry, coating (painting, co-extrusion), off shore, wire and cable.

Compliance

This product is ANSI/NSF Standard 61 certified.

Other

The key features are: Additive: Heat stabilizer, barrier resin, chemical resistant, heat stabilized, high purity, homopolymer, light stabilized, paintable, UV resistant UV stabilized

Processing methods

Casting, coating, coextrusion, film extrusion, injection molding, sheet extrusion, thermoforming

UV resistance

Good

This material data has been provided by Goodfellow.